loading

Integral Skin System Blended Polyol

Availability:

A.Blended Polyol

ItemIndex
Material Temperature20~25℃
Mold Temperature40~50℃
Cream Time15~25s
Rising Time50~70s
POL/ ISO Ratio100:45~55

*The actual reactivity characteristics may be adjusted according to process conditions and clients’ requirements


B.ISO

BrandNCO%Details
Liquefied MDI29.5Liquefied MDI
JHW854529.9Modified MDI, good performance in integral skin